Measuring the relative permittivity of polyetherimide/(Ba_(0.8)Sr_(0.2))(Ti_(0.9)Zr_(0.1))O_(3) composites from 10 kHz to 12 GHz

机译:Measuring the relative permittivity of polyetherimide/(Ba_(0.8)Sr_(0.2))(Ti_(0.9)Zr_(0.1))O_(3) composites from 10 kHz to 12 GHz

获取原文
获取原文并翻译 | 示例
           

摘要

The relative permittivity of polyetherimide-(Ba_(0.8)Sr_(0.2))(Ti_(0.9)Zr_(0.1))O_(3) (PEI-BSTZ) composites is measured from 10 kHz to 1 MHz using plate method. As the content of BSTZ filler is less than 18 vol percent, the experimental values are fitted to the values predicted by Lichtenecker equation. As the content is more than 18 vol percent, the measured relative permittivity of PEI-BSTZ composites is higher than the predicted values. The relative permittivity of PEI-BSTZ composites is measured at 1-12 GHz using "square cavity resonator" method. Measured at gigahertz, the relative permittivity of PEI-BSTZ composites is almost unchanged.

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号