Degradation of HDPE, LLDPE, and blended polyethylene geomembranes in extremely low and high pH mining solutions at 85 °C

机译:Degradation of HDPE, LLDPE, and blended polyethylene geomembranes in extremely low and high pH mining solutions at 85 °C

获取原文
获取原文并翻译 | 示例
           

摘要

? 2023The durability of five 1.5-mm thick geomembranes (GMBs) is investigated in pH 0.5 and 13.5 synthetic mining solutions using immersion tests. Two high density polyethylene (HDPE), two linear low density polyethylene (LLDPE), and one blended polyethylene (BPO) GMBs are investigated at 85 °C for incubation durations of 4.5–6.5 years. It is shown that the degradation of all five GMBs in the high pH solution is faster than in the low pH solution. In the pH 0.5 solution, one of the HDPEs and the BPO GMBs exhibited polymer degradation before or at the time of the depletion of their antioxidants. In pH 13.5, four out of the five GMBs exhibited degradation and followed the conceptual three-stage degradation model until nominal failure. However, there is no correlation between the long-term performance of these GMBs and their resin type or their initial properties since one of the examined LLDPEs outperformed all the higher density/crystallinity GMBs with higher initial properties while the other LLDPE did not perform well. Thus, when selecting a GMB for a desired application, the relative performance of different candidate GMBs can be only assessed using immersion tests using the solutions expected in the field.

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号