Facile synthesis of luminescent and amorphous La2O3-ZrO2:Eu3+ nanofibrous membranes with robust softness

机译:简单的合成发光和非晶态La2O3-ZrO2:欧盟三国+ nanofibrous膜与健壮柔软

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Novel luminescent and amorphous La2O3-ZrO2:Eu3+ (LZE) nanofibrous membranes with robust softness are fabricated for the first time via a facile electrospinning technique. By incorporating zirconium oxide, the as-prepared lanthanum oxide nanofibrous membranes can be dramatically changed from extreme fragility to robust softness. Meanwhile, the softness and luminescent performance of LZE nanofibrous membranes can be finely controlled by regulating the doping concentration of zirconium oxide and europium in lanthanum oxide nanofibers. Additionally, the crystal structure analysis using X-ray diffractometer and high resolution transmission electron microscopy measurements have confirmed the correlation between the amorphous structure and softness. Furthermore, LZE membranes show the characteristic emission of Eu3+ corresponding to D-5(0,1, 2)-F-7(0,1,2,3,4) transitions due to an efficient energy transfer from O2- to Eu3+. The LZE nanofibrous membranes with the optimum doping Eu3+ concentration of 3 mol% exhibit excellent softness and luminescent properties, which make the materials to have potential applications in fluorescent lamps and field emission displays.
机译:新颖的发光和无定形La2O3-ZrO2:欧盟三国+(LZE) nanofibrous膜与健壮的柔软装配式首次通过简单吗电纺的技术。氧化锆,和氧化镧nanofibrous膜可以极大地改变了从极端脆弱健壮的柔软。与此同时,柔软和发光的性能LZE nanofibrous膜精确控制通过调节掺杂氧化锆和铕的浓度氧化镧纳米纤维。使用x射线晶体结构分析衍射仪和高分辨率的传播电子显微镜测量证实无定形结构之间的相关性和柔软。欧盟三国+相应的排放特征D-5 (0, 1, 2) -F-7(0, 1, 2, 3, 4)由于一个过渡有效的能量转移从O2 -欧盟三国+。LZE nanofibrous膜最佳掺杂欧盟三国+浓度3 mol %展览优秀柔软和发光性能,使材料中有潜在的应用荧光灯和场致发射显示器。

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号