The purpose of this study was to measure the shear bond strength of stainless steel brackets bonded to enamel in vitro with a recently developed self-etching primer (Transbond Plus Self Etching Primer, 3M Unitek, Monrovia, Calif). Forty-eight extracted human teeth were obtained and randomly divided into 4 groups of 12: (1) control group with a conventional etchant and separate primer, (2) experimental group with the self-etching primer, left for 15 seconds before bonding, (3) same as group 2, but with the primer left for 2 minutes before bonding, (4) same as group 2, but with the primer left for 10 minutes before bonding. For each group, stainless steel brackets were mounted onto the prepared enamel, stored for 24 hours at 37 degrees C, and tested in a testing machine with a crosshead speed of 1 mm/min. There was no significant difference in the bond strength between the 4 groups as determined by analysis of variance (ANOVA) (P <.05). Under the conditions of these experiments, a 10-minute delay in bonding after application of the self-etching primer might not be deleterious to adhesion.
机译:这项研究的目的是使用最近开发的自蚀刻底漆(Transbond Plus自蚀刻底漆,3M Unitek,蒙罗维亚,加利福尼亚州)测量与牙釉质体外粘结的不锈钢托架的剪切粘结强度。获得了48颗拔出的人类牙齿并将其随机分为4组,每组12组:(1)对照组使用常规蚀刻剂和单独的底漆,(2)实验组使用自蚀刻底漆,在粘结前放置15秒,( 3)与第2组相同,但在粘结前需留底漆2分钟;(4)与第2组相同,但在粘结前需留底漆10分钟。对于每组,将不锈钢托架安装到准备的瓷釉上,在37摄氏度下保存24小时,并在测试机中以1 mm / min的十字头速度进行测试。通过方差分析(ANOVA)确定,四组之间的粘合强度没有显着差异(P <.05)。在这些实验的条件下,在施加自蚀底漆后,粘合延迟10分钟可能不会对粘合产生有害影响。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号