Serpentinic laterite ore, after suitable mineral processing operations as described in Part I, was subjected to heap as well as atmospheric agitation leaching. The heap leach results showed that serpentinic laterites can be leached by this technique. The nickel and cobalt recoveries achieved were 60 percent and 45 percent, respectively, in 10 days. The sulphuric acid consumption amounted to 40 kg H_2SO_4/kg Ni. However, the effectiveness of leaching depended on the calcite content of the ore as this adversely affected the permeability of the heap. The agitation leach tests showed that the ore could be leached at atmospheric pressure without problems. Recoveries achieved were up to 74 percent for nickel and 51 percent for cobalt, after 2 h of leaching. The sulphuric acid consumption, depending on conditions, averaged 55 kg/kg Ni. Pulp mixing and filtration were excellent.
机译:在按照第I部分所述进行适当的矿物加工操作之后,对蛇纹岩红土矿进行堆浸和大气搅拌浸出。堆浸结果表明,该技术可以浸润蛇纹岩红土。在10天内,镍和钴的回收率分别达到60%和45%。硫酸消耗量为40 kg H_2SO_4 / kg Ni。但是,浸出的有效性取决于矿石中的方解石含量,因为这会对堆的渗透性产生不利影响。搅拌浸出试验表明矿石可以在大气压下浸出而没有问题。浸出2小时后,镍的回收率高达74%,钴的回收率高达51%。根据条件,硫酸消耗量平均为55 kg / kg Ni。纸浆混合和过滤效果极佳。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号