Load-bearing characteristics of heat-treated rubberwood furniture components and joints

机译:热处理的橡胶木家具零件和接头的承重特性

获取原文
获取原文并翻译 | 示例
           

摘要

The load bearing characteristics of heat-treated rubberwood furniture components and joints were studied. It was found that heat-treated samples had significantly lower fatigue strength compared to the conventionally kiln-dried rubberwood samples, which were used as control specimens. Inevitably, the recommended allowable design stresses for heat-treated rubberwood furniture components and joints could be set at 40 and 25 % of the respective bending strengths, in order to ensure its compliance with furniture performance standards. These figures are much lower than the allowable design stresses for conventionally kiln dried components, reflecting the need for a lower safety margin when working with heat-treated materials.
机译:研究了经热处理的橡胶木家具零部件和接头的承重特性。已发现,与用作对照样品的传统窑干橡胶木样品相比,热处理后的样品具有明显更低的疲劳强度。为了确保其符合家具性能标准,不可避免地,建议将经热处理的橡胶木家具部件和接缝的推荐设计应力设为各自抗弯强度的40%和25%。这些数字远低于传统窑干部件的允许设计应力,这反映了在使用热处理材料时需要降低安全裕度的要求。

著录项

  • 来源
    《Holz als Roh- und Werkstoff》 |2013年第2期|287-289|共3页
  • 作者

    J. Ratnasingam; Florin Ioras;

  • 作者单位

    Faculty of Forestry, Universiti Putra Malaysia,43400 Serdang, Selangor, Malaysia;

    Faculty of Technology, Buckinghamshire New University,Queen Alexandra Road, 11 2 JZ High Wycombe,Buckinghamshire, UK;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号