Radiographic and ultrasonic examinations of three pipes of the Gundremmingen nuclear power plant revealed cracks with a maximum depth of about 2 mm on the inside of the pipes with a wall thickness of 7.1 mm. For continued service until replacement two representative areas were monitored for crack growth by means of the potential drop method. As crack growth during the last year of service can be excluded by metallographic examinations after replacement the result of monitoring by means of potential probes -- in relation to its resolution capacity no crack growth in the period under monitoring is confirmed. A final evaluation based on the actual crack depths results in minimum resolution of 0.2 and 0.5 mm in crack depth. The suitability of the potential drop method for in-service monitoring of existing indications for crack growth -- even until replacement of the component, if necessary could thus be demonstrated convincingly.
机译:对Gundremmingen核电站的三根管道进行射线照相和超声波检查,发现在管道内部最大深度约为2毫米的裂缝,壁厚为7.1毫米。为了继续维修直到更换为止,通过电位降法监测了两个代表性区域的裂纹扩展。由于更换后的金相检查可以排除使用服务后最后一年中的裂纹扩展,因此用潜在探针进行监测的结果-就其分辨能力而言,在监控期间未确认裂纹扩展。根据实际裂纹深度进行的最终评估得出裂纹深度的最小分辨率为0.2和0.5 mm。因此,有说服力的证明了潜在跌落法在运行中监测现有裂纹扩展迹象的适用性-即使在更换组件之前,也可以令人信服。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号