PCAs The current study aims at comparing the effect of three different process control agents (PCAs)-namely methanol (ME), ethylene glycol (EG) and stearic acid (SA)- on microstructure and mechanical properties of Al-4.4Cu-0.5Mg alloy (AA) produced by mechanical alloying of elemental powders and subsequent hot extrusion. The effect of PCAs on particle size with milling time is insignificant. The average particle size of the milled powders of all samples has reached a steady state after 3 h. Even though the grain size and its distribution in all the samples in upset-forged, hot extruded, solutionised and peak aged conditions are similar, the number density and volume fraction of nanosized theta' precipitates are observed to be higher in the case of AA-ME sample as compared to the other samples. AA-EG samples exhibited highest hardness when compared to the other samples. This can be attributed to the higher oxygen content in AA-EG sample that results in the formation of oxides that got dispersed in the matrix. Valid tensile test data was obtained only from AA-ME sample. The failure of AA-EG and AA-SA samples can be attributed to the presence of microcracks and higher oxide content. It can be concluded that nature of PCA has significant effect on oxygen pick up, size, number density and volume fraction of precipitates and in producing defect free bulk sample.
机译:目前的研究目前的研究旨在比较三种不同过程控制剂(PCAS)甲醇(ME),乙二醇(例如)和硬脂酸(SA)的效果 - Al-4.4Cu-0.5mg的微观结构和机械性能通过机械合金化元素粉末和随​​后的热挤出生产的合金(AA)。 PCA对具有研磨时间的粒径的影响是微不足道的。所有样品的碾磨粉末的平均粒径已在3小时后达到稳定状态。尽管在镦锻,热挤出,解决方案化和峰值老化条件下的所有样品中的晶粒尺寸及其分布相似,但纳米化θ'沉淀物的数量密度和体积分数在AA的情况下较高与其他样品相比,我样本。与其他样品相比,AA-例如样品在与其他样品相比时表现出最高的硬度。这可以归因于AA的较高的氧含量 - 例如样品中导致形成分散在基质中的氧化物的样品。仅从AA-ME样品获得有效的拉伸试验数据。 AA-EG和AA-SA样品的失败可归因于微裂纹和更高的氧化物含量。可以得出结论,PCA的性质对沉淀物的氧气拾取,尺寸,数量密度和体积分数具有显着影响,以及产生缺陷的散装样品。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号