Electrospun non-woven membrane of poly(ethylene covinyl alcohol) end-capped with potassium sulfonate

机译:封端有磺酸钾的聚乙烯乙烯醇电纺无纺布膜

获取原文
获取原文并翻译 | 示例
           

摘要

Electrospinning is a technique used to produce micron to submicron diameter polymeric fibers. The low density of electrospun fibers is important when considering end-use applications as use on filtration material and lightweight wings for micro-air vehicles (MAV). A polymer of poly(ethylene covinyl alcohol) end-capped with sulfonate (EVOH-g-PSN) is synthesized by sulfonification of poly(ethylene-co-vinyl alcohol) (EVOH) with 1,3-propane sultone (PSN) and characterized by Fourier transform infrared spectroscopy. The polymer is soluble in water when the ratio of hydroxyl in EVOH versus PSN is more than 2.5 and insoluble in water when the ratio is less than 2.5. The EVOH-g-PSN non-woven membrane is prepared by electrospinning and the morphology of the membrane is examined using scanning electron microscopy (SEM) to identify any conformational changes that occur due to electrospinning voltage. The molar ratio of sulfur/potassium on the EVOH-g-PSN non-woven membranes were determined using a point scanning analysis with energy dispersive X-ray spectrometer (EDS). The EDS result show that the S/K molar ratios is almost equal to 1.0 indicating that the element of sulfur and potassium in the polymer could exist as the -SO3K. The SEM shows that the high voltage makes the beaded filaments get into finer fibers. (C) 2004 Elsevier B.V. All rights reserved.
机译:电纺丝是用于生产微米至亚微米直径的聚合物纤维的技术。当考虑将最终用途用作过滤材料和微型飞机(MAV)的轻质机翼时,低密度的电纺纤维非常重要。通过用1,3-丙烷磺酸内酯(PSN)磺化聚(乙烯-共-乙烯醇)(EVOH)来合成端基为磺酸盐(EVOH-g-PSN)的聚乙烯(乙烯-乙烯醇)聚合物,并对其进行表征通过傅立叶变换红外光谱。当EVOH中的羟基与PSN的羟基比例大于2.5时,该聚合物可溶于水;而当该比例小于2.5时,该聚合物则不溶于水。 EVOH-g-PSN无纺布膜通过静电纺丝制备,并使用扫描电子显微镜(SEM)检查膜的形态,以识别由于静电纺丝电压而发生的任何构象变化。 EVOH-g-PSN非织造膜上硫/钾的摩尔比使用能量色散X射线光谱仪(EDS)进行点扫描分析确定。 EDS结果表明,S / K摩尔比几乎等于1.0,表明聚合物中的硫和钾元素可能以-SO3K的形式存在。 SEM表明,高压使珠状长丝进入更细的纤维中。 (C)2004 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号