The residual lignins KRL and SRL, isolated from a conventional kraft pulp and a SuperBatch pulp respectively, were reacted with per-oxyformic acid (PFA). The reagent consumptions were determined and the products fractionated according to their solubility. Both lignins consumed a roughly equal amount of PFA, which was nearly 50% higher than that consumed by kraft lignin. The undissolved fractions of PFA-treated residual lignins (yield > 80%) contained less aromatic units, phenolic hydroxyl and methoxyl groups, and considerably more carboxyl groups (including those of formate esters) than the untreated lignins. The extent of these modifications was approximately equal for KRL and SRL, which together with the similar PFA consumptions and product yields of KRL and SRL indicates that the two residual lignins showed no essential difference in reactivity toward PFA. The effect of fiber wall morphology on delignification efficiency during PFA delignification is suggested to be small because of the cleavage of lignin-carbohydrate linkages occurring under acid conditions. The part of KRL remaining insoluble after PFA-treatment had a 40% higher molar mass than KRL while in the case of SRL there was hardly any such difference in molar mass. The lignins solubilized during the PFA treatments represented the most highly degraded part of the lignins, having very low molar masses and being richer in carboxyl groups and lower in aromatic units, phenolic hydroxyl, and methoxyl groups than the undissolved lignins.
机译:分别从常规牛皮纸浆和SuperBatch浆液中分离出的残留木质素KRL和SRL与过氧甲酸(PFA)反应。确定试剂消耗量,并根据其溶解度分级分离产物。两种木质素消耗的PFA量大致相等,比牛皮纸木质素消耗的PFA高出近50%。经PFA处理的残留木质素的未溶部分(收率> 80%)比未处理的木质素包含更少的芳族单元,酚羟基和甲氧基,以及更多的羧基(包括甲酸酯)。这些修饰的程度对于KRL和SRL大约相等,再加上相似的PFA消耗量和KRL和SRL的产品收率,表明两种残留的木质素对PFA的反应性没有本质上的区别。 PFA脱木质素过程中纤维壁形态对脱木质素效率的影响较小,这是因为在酸性条件下发生的木质素-碳水化合物键断裂。经PFA处理后保持不溶的KRL部分的摩尔质量比KRL高40%,而在SRL的情况下,摩尔质量几乎没有这种差异。在PFA处理过程中溶解的木质素代表了木质素降解程度最高的部分,摩尔质量非常低,羧基含量更高,芳香单元,酚羟基和甲氧基比未溶解的木质素更低。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号