Spherical micron-sized MnS-C and MnO-C composite powders are successfully prepared by post-treating the spray-dried precursor powders. Dextrin, which is used as the carbon source material, plays a key role in the preparation of the composite powders with regular morphologies; the bare MnS and MnO powders prepared from the spray solution without dextrin have irregular morphologies. The MnS-C composite powders prepared from the spray solution containing 17 g L-1 of dextrin have mixed crystal structures of alpha- and gamma-MnS phases. These powders exhibit superior electrochemical properties compared with those of their MnS and MnO-C counterparts. For example, at a current density of 0.5 A g(-1), the MnO-C powders have a 100th-cycle discharge capacity of 321 mA h g(-1); the corresponding discharge capacities of the MnS powders prepared from spray solutions containing 0, 17, and 50 g L-1 of dextrin are 501, 786, and 636 mA h g(-1), respectively. (C) 2015 Elsevier B.V. All rights reserved.
机译:通过对喷雾干燥的前体粉末进行后处理,成功制备了球形微米级MnS-C和MnO-C复合粉末。用作碳源材料的糊精在制备规则形貌的复合粉末中起着关键作用。由不含糊精的喷雾溶液制备的裸露的MnS和MnO粉末具有不规则的形貌。由包含17克L-1糊精的喷雾溶液制备的MnS-C复合粉末具有α-和γ-MnS相的混合晶体结构。与它们的MnS和MnO-C对应物相比,这些粉末具有优异的电化学性能。例如,在电流密度为0.5 A g(-1)时,MnO-C粉末的第100次循环放电容量为321 mA h g(-1)。由含有0、17和50 g L-1糊精的喷雾溶液制备的MnS粉末的相应放电容量分别为501、786和636 mA h g(-1)。 (C)2015 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号