Crystallization Behavior and Dynamic Mechanical Properties of Poly(L-Lactic Acid) with Poly(Ethylene Glycol) Terminated by Benzoate

机译:苯甲酸酯封端的聚乙二醇乙二醇的结晶行为和动态力学性能

获取原文
获取原文并翻译 | 示例
           

摘要

Effect of the addition of poly(ethylene glycol) terminated by benzoate (PEG-BA) on the crystallization behavior and dynamic mechanical properties of poly(L-lac-tic acid) PLLA is studied as compared with poly(ethylene glycol) (PEG-OH). It is found that PEG-BA is miscible with PLLA and shows good plasticizing effect. Because PEG-OH having the same degree of polymerization is immiscible with PLLA, the end group in PEG-BA, i.e., benzoate, plays an important role in the miscibility. Furthermore, PEG-BA does not induce the PLLA degradation at melt-processing, whereas PEG-OH leads to the hydrolysis degradation. Finally, the addition of PEG-BA pronounces the crystallization rate of PLLA at low crystallization temperatures and thus enhances the degree of crystallinity at conventional processing. Consequently, the temperature dependence of dynamic mechanical properties are similar to that for iso-tactic polypropylene.
机译:与聚乙二醇(PEG-BA)相比,研究了添加苯甲酸酯(PEG-BA)封端的聚乙二醇对聚(L-乳酸)PLLA结晶行为和动态力学性能的影响。哦)。发现PEG-BA可与PLLA混溶并显示出良好的增塑效果。由于具有相同聚合度的PEG-OH与PLLA不混溶,因此PEG-BA中的端基(即苯甲酸酯)在混溶性中起重要作用。此外,PEG-BA在熔融加工时不引起PLLA降解,而PEG-OH导致水解降解。最后,PEG-BA的加入表明低结晶温度下PLLA的结晶速率,因此提高了常规加工中的结晶度。因此,动态力学性能的温度依赖性类似于等规聚丙烯。

著录项

  • 来源
    《Journal of Polymers and the Environment》 |2014年第2期|183-189|共7页
  • 作者单位

    School of Materials Science, Japan Advanced Institute of Science and Technology, 1-1 Asahidai, Nomi, Ishikawa 923-1292, Japan;

    School of Materials Science, Japan Advanced Institute of Science and Technology, 1-1 Asahidai, Nomi, Ishikawa 923-1292, Japan;

    School of Materials Science, Japan Advanced Institute of Science and Technology, 1-1 Asahidai, Nomi, Ishikawa 923-1292, Japan;

    School of Materials Science, Japan Advanced Institute of Science and Technology, 1-1 Asahidai, Nomi, Ishikawa 923-1292, Japan;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    Poly(lactic acid); Plasticization; Crystallization; Hydrolysis degradation;

    机译:聚乳酸增塑结晶;水解降解;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号