The present work aims to evaluate the photocatalytic activity of photo-TiCb from various producers (Evonik, Kemira, Kronos, Millennium, Sachtleben and Tayca), in the form of powder pressed films and upon incorporation in a water-based paint, for outdoor NO abatement. The photocatalytic activity of the different samples was evaluated in terms of NO conversion and selectivity towards nitrite and nitrate ions following approximately the ISO 22197-1:2007(E) standard. The highest yields obtained for powder pressed films were achieved with VLP7000 (0.70), followed by VLP7101 (0.55) and UVLP7500 (0.55), all from Kronos. On the other hand, when incorporated in paint films, the highest yields were obtained with PC500 and PC105 from Millennium and UV100 from Sachtleben {ca. 0.15). The paint matrix plays an important role on the photocatalytic activity. In particular, the time for steady state is one or two orders of magnitude higher when the photocatalysts are incorporated in paint films in relation to the powder pressed films. The paint films were activated following the procedure recommended by the above-mentioned standard. However, the photocatalytic activity of films incorporating P2S (Evonik) was displayed only when higher power radiation and higher humidity conditions were used. This allowed for similar levels of photocatalytic activity as the other paint films.
机译:本工作旨在评估粉末压制薄膜形式并掺入水性涂料中用于室外NO的各种生产商(赢创,凯米拉,克罗诺斯,千禧,萨奇本和泰卡)生产的光TiCb的光催化活性。减排。遵循ISO 22197-1:2007(E)标准,根据NO转化率和对亚硝酸根和硝酸根离子的选择性评估了不同样品的光催化活性。使用VLP7000(0.70),其次是VLP7101(0.55)和UVLP7500(0.55)获得粉末压制薄膜的最高产量,所有这些均来自Kronos。另一方面,当掺入漆膜中时,Millennium的PC500和PC105以及Sachtleben的UV100获得最高的收率。 0.15)。涂料基质对光催化活性起重要作用。特别地,当相对于粉末压制膜将光催化剂掺入漆膜中时,稳态时间要高一个或两个数量级。按照上述标准推荐的步骤活化漆膜。但是,仅在使用较高功率的辐射和较高湿度的条件下,才能显示掺有P2S的薄膜的光催化活性(赢创)。这允许与其他漆膜相似水平的光催化活性。

著录项

  • 来源
    《Journal of Environmental Management》 |2011年第7期|p.1724-1732|共9页
  • 作者单位

    LEPAE — Departamento de Engenharia Quimica, Faculdade de Engenharia - Universidade do Porto, Rua Dr. Roberto Frias s, Porto 4200-465, Portugal;

    LEPAE — Departamento de Engenharia Quimica, Faculdade de Engenharia - Universidade do Porto, Rua Dr. Roberto Frias s, Porto 4200-465, Portugal;

    LEPAE — Departamento de Engenharia Quimica, Faculdade de Engenharia - Universidade do Porto, Rua Dr. Roberto Frias s, Porto 4200-465, Portugal;

  • 收录信息 美国《科学引文索引》(SCI);美国《化学文摘》(CA);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    NO_X; photocatalysis; TiO_2; paint films; powder pressed films;

    机译:NO_X;光催化;TiO_2;漆膜;粉末压膜;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号