Tensile Deformation and Rotating-Bending Fatigue Properties of a Highelastic Thin Wire, a Superelastic Thin Wire, and a Superelastic Thin Tube of NiTi Alloys

机译:NiTi合金高弹细线,超弹细线和超弹细管的拉伸变形和旋转弯曲疲劳特性

获取原文
获取原文并翻译 | 示例
           

摘要

The tensile deformation and rotating-bending fatigue properties of a highelastic thin wire, a superelastic thin wire and a superelastic thin tube, all made of NiTi alloys, were investigated experimentally. The results obtained are summarized as follows: (I) The stress-strain curve of the highelastic thin wire is approximately linear up to a strain of 4 percent with a stress of 1400 MPa and shows little dependency' on temperature and strain rate; (2) The modulus of elasticity for the initial loading stage of both the highelastic wire and the superelastic tube is low, showing superior bending flexibility as is necessary for medical applications; (3) The slopes of the strain-life curves of the alloys are steep in the low-cycle fatigue region (the strain amplitude of the fatigue limit is in the region of 0.6-0.8 percent); and (4) In the tube, fatigue cracking initiates on the rougher inner surface, resulting in a shorter fatigue life than in the case of the wire.
机译:实验研究了均由NiTi合金制成的高弹细线,超弹细线和超弹细管的拉伸变形和旋转弯曲疲劳性能。得出的结果概括如下:(I)高弹性细线的应力-应变曲线在应力为1400 MPa时,应变达到4%时大致呈线性,对温度和应变率的依赖性很小。 (2)高弹力线材和超弹力管的初始加载阶段的弹性模量低,显示出优异的弯曲柔韧性,这是医疗应用所必需的; (3)在低周疲劳区域,合金的应变寿命曲线的斜率陡峭(疲劳极限的应变幅度在0.6%至0.8%的范围内); (4)在管内,在较粗糙的内表面上产生疲劳裂纹,与金属丝相比,疲劳寿命短。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号