Five coals of different rank and of different content of sulphur were subjected to oxidation by peroxyacetic acid (PAA), 5% nitric acid, by oxygen in 0.5N Na_2CO_3 aqueous solution and the air oxidation for 7 days at 125℃. The processes of oxidation were carried out for coal samples demineralised by the Radmacher method, and additionally for the pyrite-free coal samples. Proximate, elemental and spectral analyses of the initial coals and the products obtained from them were made. The most effective oxidising agents were 5% HNO_3 and PAA. As a result of oxidation, a significant part of the organic components of coal is converted into acid soluble products. Depending on the oxidising agent, the loss of sulphur in the solid oxidation products was different and the highest for the coal samples oxidised with HNO_3 and PAA. Formation of oxidised sulphur species (S=O and ―SO_2) was detected by IR spectroscopy. FTIR data also provide useful information on evolution of the molecular structure of different rank coals on oxidation, in particular in the carbonyl and aliphatic ranges (1800―1500 and 3500―2800 cm~(-1)).
机译:用过氧乙酸(PAA),5%硝酸,0.5N Na_2CO_3水溶液中的氧气对五种不同等级和不同硫含量的煤进行氧化,然后在125℃下空气氧化7天。对于通过Radmacher方法脱矿的煤样品,以及不含黄铁矿的煤样品,都进行了氧化过程。对初始煤和从中获得的产物进行了近,元素和光谱分析。最有效的氧化剂是5%HNO_3和PAA。氧化的结果是,煤炭的大部分有机成分被转化为酸溶性产物。取决于氧化剂,固体氧化产物中硫的损失是不同的,并且被HNO_3和PAA氧化的煤样品中硫的损失最高。通过红外光谱检测到氧化的硫物质(S = O和-SO_2)的形成。 FTIR数据还提供了有关不同等级煤在氧化作用下的分子结构演变的有用信息,特别是在羰基和脂族范围(1800-1500和3500-2800 cm〜(-1))中。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号