机译:在不同的固液比和固化温度下制备的粉煤灰和残留的稻壳粉煤灰基地质聚合物的性能和微观结构特征
Department of Civil and Construction Engineering, National Taiwan University of Science and Technology, Taipei, 10607 Taiwan, Republic of China,Department of Rural Technology, Can Tho University, Ninh Kieu District, Can Tho City 900000, Vietnam;
Department of Civil and Construction Engineering, National Taiwan University of Science and Technology, Taipei, 10607 Taiwan, Republic of China;
Department of Environmental Engineering, National Ilan University, I-Lan, 26047 Taiwan, Republic of China;
geopolymer; fly ash; rice husk ash; solid-to-liq-uid ratio; curing temperature;
机译:碱活化剂和稻壳灰分含量对粉煤灰和残余稻壳灰基地质聚合物强度发展的影响
机译:Na_2O / SiO_2摩尔比,固化温度和时效对碱活化粉煤灰基地质聚合物抗压强度,形态和微观结构的影响
机译:高温曝光和预测其残余抗压强度环境固化和热固化粉煤灰地质混凝土的劣化
机译:NaOH摩尔分数,Na2SiO3 / NaOH比,粉煤灰/碱性活化剂比和固化温度与粉煤灰基地质聚合物强度的关系
机译:粉煤灰基地质聚合物的比例,性能评价及其在工程复合材料中的应用
机译:用响应面方法在增强稻壳灰基地缘聚合物复合涂料中的响应表面方法优化粘合强度和微观结构性能
机译:升高温度对高体积粉煤灰基岩岩混凝土机械性能的影响,砂浆及浆料在室温下固化