Titanium dioxide (TiO 2 ) nanotubes obtained by the anodic oxidation of titanium metal foils can be used for the photocatalytic degradation of organic pollutants. The aim of our study was to determine the influence of the titanium foil’s surface treatment on the final morphology of the TiO 2 nanotubes and their photocatalytic activity. In our experiments, we used two different titanium foils that were electropolished or untreated prior to the anodic oxidation. The morphologies of the starting titanium foils and the resulting TiO 2 nanotube layers were investigated and the photocatalytic activities measured by the decomposition of caffeine under UV irradiation. Our results showed that electropolishing of the starting foils produced a more uniform and smoother TiO 2 nanotubes surface. In contrast, the TiO 2 nanotube surfaces from untreated titanium foils mimic the initial surface roughness of the titanium foil. A comparison of the photocatalytic properties of the TiO 2 nanotube layers obtained from the untreated and electropolished titanium foils showed that electropolishing does not necessarily improve the photocatalytic properties of the resulting TiO 2 nanotube layer. It was found that the determining factors influencing the photocatalytic activity are the chemical impurities (Ti-nitride) on the surface of the titanium foils and the surface roughness of the TiO 2 nanotube layer. The highest photocatalytic activity was achieved with the anodized untreated foil with the minimal presence of Ti-nitride and a relatively high roughness of the TiO 2 nanotubes.
机译:通过氧化钛金属箔的阳极氧化获得的二氧化钛(TiO 2)纳米管可用于有机污染物的光催化降解。我们的研究目的是确定钛箔表面处理对TiO 2纳米管的最终形态的影响及其光催化活性。在我们的实验中,我们在阳极氧化之前使用了两种不同的钛箔,该钛箔在阳极氧化之前被电抛光或未治疗。研究了起始钛箔和所得TiO 2纳米管层的形态学,并通过紫外线照射下咖啡因分解测量的光催化活性。我们的研究结果表明,电抛光的起始箔产生了更均匀和更平滑的TiO 2纳米管表面。相反,来自未处理钛箔的TiO 2纳米管表面模拟了钛箔的初始表面粗糙度。从未处理和电抛光钛箔获得的TiO 2纳米管层的光催化性质的比较表明,电抛光不一定改善所得TiO 2纳米管层的光催化性质。发现影响光催化活性的确定因子是钛箔表面上的化学杂质(Ti-氮化物)和TiO 2纳米管层的表面粗糙度。用阳极氧化未处理的箔在Ti-氮化物的最小存在和TiO 2纳米管的相对高粗糙度下实现最高的光催化活性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号