Aim: To evaluate the effect of storage media and autoclaving on shear bond strength of composite to enamel. Materials and Methods: 100 human premolars were randomly divided into ten groups of ten as follows: C: freshly extracted teeth. A: Autoclaved freshly extracted teeth. CH-6: 6 month storage in 0.5 % chloramine T. CA-6: 6 month storage in 0.5 % chloramine T + autoclaving. T-6: 6 month storage in 0.04 % thymol. TA-6: 6 month storage in 0.4% thymol + autoclaving. Ch-12:12 month storage in 0.5 % chloramine T. CA-12: 12 month storage in 0.5 % chloramine T + autoclaving. T-12: 12 month storage in 0.4% thymol. TA-12:12 month storage in 0.4% thymol + autoclaving. One composite cylinder was bonded on each specimen for evaluation of shear bond strength (SBS) and failure modes. Data were analyzed using three-way ANOVA, Tukey’s post hoc and Chi square tests and the level of significance was set at P= 0.05. Results: Autoclaving and storage media had no significant effect on SBS (P-value = 0.818 for storage media and P-value = 0.221 for autoclaving). However, storage duration significantly changed SBS (P-value = 0.00). There were no correlations among the variables (P-value > 0.05). Storage media and duration had no significant effect on failure modes (P-value > 0.05), but autoclaving significantly increased cohesive failure of enamel (P-value =0.039). Conclusion: Storage of teeth in chloramine T and thymol had no significant effect on bond strength to enamel. Although autoclaving of specimens may not alter bond strength, it can significantly increase the cohesive failure of enamel.
机译:目的:评估储存介质和高压灭菌对复合材料与瓷釉的剪切粘结强度的影响。材料与方法:将100颗人类前磨牙随机分为10组,每组10条,如下所示:C:新鲜拔牙。答:高压灭菌的新鲜拔牙。 CH-6:在0.5%的氯胺T中保存6个月。CA-6:在0.5%的氯胺T中+保存6个月。 T-6:在0.04%百里酚中储存6个月。 TA-6:在0.4%百里酚+高压灭菌中保存6个月。将Ch-12:12个月储存在0.5%的氯胺T中。CA-12:将12个月储存在0.5%的氯胺T中+高压灭菌。 T-12:在0.4%百里酚中储存12个月。 TA-12:12个月以0.4%百里酚+高压灭菌保存。将一个复合圆柱体粘结在每个样品上,以评估剪切粘结强度(SBS)和破坏模式。使用三向方差分析,Tukey事后检验和卡方检验分析数据,显着性水平设置为P = 0.05。结果:高压灭菌和存储介质对SBS没有显着影响(存储介质的P值= 0.818,高压灭菌的P值= 0.221)。但是,存储时间显着改变了SBS(P值= 0.00)。变量之间没有相关性(P值> 0.05)。存储介质和持续时间对破坏模式没有显着影响(P值> 0.05),但高压灭菌处理显着增加了搪瓷的内聚破坏性(P值= 0.039)。结论:在氯胺T和百里酚中储存牙齿对牙釉质的粘结强度没有显着影响。尽管对样品进行高压灭菌不会改变粘结强度,但会显着增加搪瓷的内聚力。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号