After a severe fire, concrete structures are generally capable of being repaired rather than demolished. To determine whether the fire-damaged structure can be repaired, an assessment of structural integrity must be conducted. In this research, a laboratory assessment of fire-damaged reinforced concrete (RC) slabs was carried out by using Destructive Testing (DT) and Non-Destructive Testing (NDT) techniques. The study aimed to evaluate the depth of damaged concrete in RC slabs exposed to fire for different periods of time (30, 60, 90 and 120 minutes) based on the correlation between the experimental results of DT and NDT methods. The experiment was conducted with two concrete grades of 24 and 35 MPa. Limestone aggregates were used in this study. The experimental results indicated that 30 minutes of heating time did not show severe effects on reinforced concrete slabs in comparison with the other cases. A damaged concrete layer of 30 – 45 mm was observed for slabs exposed to fire in 60 and 90 minutes. Besides, 24 MPa slabs also showed a lower damage level compared with 35 MPa slabs.
机译:发生严重火灾后,混凝土结构通常能够维修而不是拆除。为了确定是否可以修复失火的结构,必须对结构完整性进行评估。在这项研究中,通过使用破坏性测试(DT)和非破坏性测试(NDT)技术对受损的钢筋混凝土(RC)板进行了实验室评估。该研究旨在根据DT和NDT方法的实验结果之间的相关性,评估在不同时间段(30、60、90和120分钟)着火的RC楼板中受损混凝土的深度。该实验是使用24和35 MPa的两种混凝土等级进行的。在这项研究中使用了石灰石骨料。实验结果表明,与其他情况相比,加热时间30分钟对钢筋混凝土板没有显示出严重的影响。在60和90分钟内暴露于火中的楼板观察到损坏的30-45毫米混凝土层。此外,24 MPa平板的破坏水平也低于35 MPa平板。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号