Introduction: The purpose of this study was to evaluate the fracture resistance of most used three preparation techniques applied laminate veneers made with three different restoration methods. Materials and Methods: 195 same sized maxillary central incisor teeth were grouped 10 different groups randomly. (testing groups n=20, control group n=15) Three different preparation techniques used for teeth preparation which were feather-edge, insical overlap and window. Laminate veneers were produced with three different methods that direct, indirect technique, and CAD/CAM milling. Control group was chosen from untreated teeth. Universal testing machinewas used for fracture resistance test. Data were analyzed with two-ways ANOVA and Tukey LSD. Results: According to results, statistically differences were found between all groups.(p<0,05) Combination of insical overlap preparation and direct technique has higher fracture resistance values than other groups.(563,9 N). Conclusions: Preparation and restoration techniques are important for fracture resistance of laminate veneers.
机译:简介:这项研究的目的是评估使用三种不同修复方法制成的层压板的最常用的三种制备技术的抗断裂性。材料与方法:将195颗相同尺寸的上颌中切牙随机分为10组。 (测试组n = 20,对照组n = 15)三种用于牙齿制备的制备技术是羽缘,异形重叠和窗口。层压贴面采用直接,间接技术和CAD / CAM铣削三种不同方法生产。对照组选自未经治疗的牙齿。万能试验机用于抗断裂试验。使用双向方差分析和Tukey LSD分析数据。结果:根据结果,各组之间存在统计学差异。(p <0,05)直插叠合和直接技术相结合具有比其他组更高的抗断裂性值(563,9 N)。结论:制备和修复技术对于层压板的抗断裂性能很重要。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号