首页> 外文期刊>Archives of Metallurgy and Materials >Microstructure and Plastic Properties of Mg-Li Alloys Smelted in Vacuum Induction Furnaces after Hot Working
【24h】

Microstructure and Plastic Properties of Mg-Li Alloys Smelted in Vacuum Induction Furnaces after Hot Working

机译:热加工后在真空感应炉中熔炼的Mg-Li合金的组织和塑性

获取原文
           

摘要

The paper analyses the characteristics of plasticity and microstructure of magnesium alloys with lithium meant for hot plastic working with different lithium content. The alloys were prepared in conditions of vacuum smelting. Achieved ingots were subject to hot extrusion. Tests on Gleeble simulator were conducted to assess the susceptibility of tested alloys to plastic forming in conditions of hot plastic working. For tested alloy the activation energy was marked for hot plastic deformation and plasticity characteristics in function of Zener-Hollomon parameter. After the analysis of the influence of temperature on the deformability of tested alloys it was stated that the alloy containing 8%Li (LAZ831) has better susceptibility to plastic treatment than alloy containing 4%Li (LAZ431), but higher than in case of classic magnesium alloys - AZ31.
机译:本文分析了含锂的镁合金的塑性和显微组织的特性,这些锂合金适用于不同锂含量的热塑料加工。该合金是在真空熔炼条件下制备的。将获得的铸锭进行热挤压。在Gleeble模拟器上进行了测试,以评估在热塑性加工条件下被测合金对塑性成形的敏感性。对于测试的合金,标记的活化能为热塑性变形和可塑性特性的齐纳霍洛蒙参数的函数。在分析温度对被测合金的可变形性的影响后,研究表明,含8%Li的合金(LAZ831)比含4%Li的合金(LAZ431)具有更好的塑性处理敏感性,但高于经典合金。镁合金-AZ31。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号