摘要

The effectiveness of natural clay, calcium phosphate, poultry manure and rice husks as cheap and ecologically non-invasive amendments for immobilizing Cu and Pb in contaminated soil was assessed. A moderately contaminated soil was sampled from a cultivated field in the vicinity of an active waste dump, characterized and amended with the immobilizing agents at 5 to 20% w/w. Single (calcium nitrate), sequential (optimized European Communities Bureau of Reference, BCR method) and kinetic (ethylenediaminetetraacetic acid, EDTA) leaching tests were performed before and after soil amendments. Single extractions showed that metal immobilization efficiencies, E were generally high (20 ≤ E ≤ 81%), increased as the agent dose and varied in the order: phosphate natural clay poultry manure rice husks. BCR extractions showed that the agents attenuated Cu and Pb mobilities and induced changes in their fractionation patterns as most of the hitherto mobile fractions became associated with the less bioavailable forms. Two metal forms: readily labile and less labile, with apparent leaching rates k1 (10-2 min-1) and k2 (10-3 min-1), respectively were identified by fitting EDTA leaching data into a two-first-order model. The immobilizing agents suppressed both k1 and k2 for Cu and only k2 for Pb. These agents may reduce risks resulting from Cu and Pb contamination in soil since metal mobility is related to its bioavailability.
机译:评估了天然粘土,磷酸钙,家禽粪便和稻壳作为便宜且生态无害的改良剂的有效性,这些改良剂用于将铜和铅固定在受污染的土壤中。从一个活跃的垃圾场附近的耕地中取样一个中等污染的土壤,用固定剂以5至20%w / w进行表征和修正。在改良土壤前后,分别进行了一次(硝酸钙),连续(优化的欧洲共同体参考局,BCR方法)和动力学(乙二胺四乙酸,EDTA)浸出试验。单次萃取表明,金属固定效率E通常很高(20≤E≤81%),随着药剂剂量的增加而增加,并且顺序依次为:磷酸盐>天然粘土>家禽粪便>稻壳。 BCR提取显示,由于大多数迄今为止可移动的馏分与生物利用度较低的形式相关,因此这些试剂减弱了Cu和Pb的迁移率,并诱导了其馏分模式的变化。通过将EDTA浸出数据拟合到一阶二阶模型中,可以识别出两种金属形式:易不稳定和不稳定,分别具有明显的浸出率k1(10-2 min-1)和k2(10-3 min-1)。 。固定剂对Cu抑制了k1和k2,对Pb抑制了仅k2。由于金属的迁移率与其生物利用度有关,因此这些试剂可以减少土壤中的铜和铅污染所致的风险。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号