This work investigated the effects of incorporating palm kernel shells (PKS) as partial replacement of coarse aggregates in hot mix asphaltic binder course. All the volumetric properties and the physical properties of the asphalt mixture were evaluated in order to determine the potential of PKS in the production of binder course for medium-trafficked roads. Percentages of PKS content rates used were 0%, 30%, 50%, 70% and 100% by weight of total coarse aggregate size of 4-8 mm. Specifically, 15 samples for control mix and 60 samples for the PKS proportions of compacted asphaltic mixture were prepared by using Marshall mixing procedure. The samples were prepared by varying bitumen content from 4.5% to 6.5% and tested using the Marshall Method.The results of control samples and PKS-incorporated samples showed effective PKS content at 50% replacement having 5.7% optimum bitumen content. Overall, it is established that PKS is a viable agriculture waste product that can be used as coarse aggregates at a specific percentage in the production of asphaltic binder course for light to medium-trafficked roads.
机译:这项工作研究了掺入棕榈仁壳(PKS)作为热拌沥青粘合剂层中部分粗骨料的替代效果。对沥青混合料的所有体积特性和物理特性进行了评估,以确定PKS在中型人行道的粘合剂层生产中的潜力。所使用的PKS含量百分比为4-8 mm的总粗骨料重量的0%,30%,50%,70%和100%。具体地,通过使用马歇尔混合程序制备了用于对照混合物的15个样品和用于压实的沥青混合物的PKS比例的60个样品。通过将沥青含量从4.5%更改为6.5%来制备样品,并使用马歇尔方法进行测试。对照样品和掺入PKS的样品的结果表明,有效的PKS含量在50%置换时具有5.7%的最佳沥青含量。总体而言,已确定PKS是一种可行的农业废品,可以在轻到中型道路的沥青粘合剂层的生产中以特定百分比用作粗骨料。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号