Stabilization of Lateritic Soil with Cassava Peels Ash

机译:木薯去皮灰稳定红土

获取原文
           

摘要

This research is aimed at assessing the impact of Cassava Peels Ash (CPA) on the stabilization of lateritic soil deposit found within Osogbo Local Government Area in Osun State, Nigeria. This project was carried out to study the characteristics of Cassava Peels Ash (CPA) stabilization on lateritic soil. Preliminary tests were performed on three samples, L1, L2, and L3 for identification and classification purposes followed by the consistency limit tests. Geotechnical property tests (compaction, California bearing ratio (CBR), and Unconfined Compression Test) were also performed on the samples, both at the stabilized and unstabilized states by adding 2, 4, 6, 8 and 10% Cassava Peels Ash (CPA) by weight of sample to the soils. The results showed that the addition of CPA improved the strengths of the samples. Optimum moisture contents (OMC) reduced to 14.58, 18.40 and 16.00% at 6, 4 and 6% CPA additions in samples L1, L2 and L3 respectively while maximum dry density (MDD) increased to 1470, 1410 and 1440 kg/m3 at 10, 4 and 2% CPA additions in samples L1, L2, and L3. The unsoaked CBR values of samples increased from 7.89 to 19.40% at 8% CPA stabilization for sample L1, for sample L2, it increases from 5.80 to 27.02% at 10% CPA stabilization and for sample L3 at the natural state, it increases from 14.50 to 18.20% at 4%. The shear strengths of samples L1, L2 and L3 also increased from 123.70 to 590.58 kN/m2 at 2% CPA stabilization, 293.48 to 297.67 kN/m2 at 10% CPA stabilization and 153.99 to 554.02 kN/m2 respectively. It was therefore concluded that Cassava Peels Ash has a good potential for stabilizing lateritic soil.
机译:这项研究旨在评估木薯果皮灰(CPA)对尼日利亚奥森州Osogbo地方政府区域内发现的红土土壤沉积物稳定性的影响。该项目旨在研究红土土壤上木薯皮灰的稳定性。为了识别和分类目的,对三个样本L1,L2和L3进行了初步测试,然后进行了一致性极限测试。还通过添加2%,4%,6%,8%和10%的木薯果皮灰(CPA)对样品进行了岩土性能测试(压实,加利福尼亚承载比(CBR)和无侧限压缩测试),分别处于稳定状态和不稳定状态。 ),以样品对土壤的重量计。结果表明,添加CPA可以提高样品的强度。在分别添加L1,L2和L3的CPA中,分别以6%,4和6%的CPA最佳含水量(OMC)降低到14.58%,18.40和16.00%,而最大干密度(MDD)分别提高到1470、1410和1440 kg / m3样品L1,L2和L3中的CPA添加量分别为10%,4%和2%。样品L1的CPA稳定度为8%时,样品的未浸泡CBR值从7.89增加到19.40%,样品L2的CPA稳定度为10%时样品的未浸透CBR值从7.80%增加到27.02%。它从4%的14.50%增加到18.20%。样品L1,L2和L3的剪切强度在CPA稳定度为2%时也从123.70增加到590.58 kN / m2,在CPA稳定度为10%时也为293.48到297.67 kN / m2,从153.99到554.02 kN / m2也增加了。因此得出结论,木薯果皮灰具有稳定红土土壤的良好潜力。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号