To demonstrate the ability of the lead isotope signature technique to evidence the spatial extent of an industrial Pb deposition plume at a local scale, dry deposition of lead in the urban environment of a Pb-Zn refinery was investigated, as a study case, using transient ("short-lived") isotopic signatures of the industrial source. Sampling campaigns were achieved in representative weather conditions, on an 8-h basis. Dry deposition rates measured downwind from refinery emissions (approximate to10(2)-10(3) mug Pb m(-2) h(-1)), cross-sectionally in a 3-5 km radius area around the plant, represent 10-100 times the urban background dry fallout, measured upwind, as well as fallout measured near other potential sources of anthropogenic Pb. The Pb-Zn refinery isotopic signature (approx. 1.100
机译:为了证明铅同位素标记技术在局部规模上证明工业Pb沉积羽流的空间范围的能力,作为研究案例,使用瞬态方法研究了Pb-Zn精炼厂城市环境中铅的干法沉积。 (“短暂”)工业来源的同位素特征。在有代表性的天气条件下,每8小时进行一次采样活动。沿炼厂排放顺风测量的干沉降速率(约10(2)-10(3)杯Pb m(-2)h(-1)),在工厂周围3-5 km半径区域中的横断面表示为10 -100倍于市区本底的干燥沉降量,是上风测量的,以及在其他可能的人为铅源附近测得的沉降量。通过与执行人员达成协议,在采样之前和现场实验期间使用相同的铅和锌矿石组进行两天的测试,可以识别铅锌精炼厂的同位素特征(约1.100

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号