Reducibility is a parameter which describes the ability of oxygen, combined with iron, to be removed from iron ore sinters by a reducing gas used in a blast furnace, and is often characterized by a Fe2+ content in a sinter. In sinters, iron at Fe2+ valence can occur in various types of minerals, which differ in values of reducibility. The set of sinters with the reducibility from 0.63%/min to 1.49%/min, prepared in the different laboratory conditions, were examined in terms of their mineral composition. The quantitative dependences between the fractions of the individual mineral constituents of the sinters and the values of reducibility were sought. The increase of the reducibility was correlated with a decrease of the content of magnetite and a rise of the fraction of hematite.
机译:可还原性是描述氧与铁结合的能力的参数,该氧与铁的结合能力是通过高炉中使用的还原性气体从铁矿石烧结矿中去除的,通常以烧结矿中的Fe2 +含量为特征。在烧结矿中,Fe2 +价态的铁可能存在于各种类型的矿物质中,这些矿物质的还原性值不同。在不同的实验室条件下制备的,还原度为0.63%/ min至1.49%/ min的一组烧结矿,根据其矿物成分进行了检查。寻找烧结矿的单个矿物成分的分数与还原性值之间的定量相关性。可还原性的提高与磁铁矿含量的减少和赤铁矿含量的增加相关。

著录项

  • 来源
    《Acta Physica Polonica》 |2016年第4期|1147-1150|共4页
  • 作者

    Krzton H.; Stecko J.; Kania Z.;

  • 作者单位

    Inst Met Zelaza, K Miarki 12-14, PL-44100 Gliwice, Poland;

    Inst Met Zelaza, K Miarki 12-14, PL-44100 Gliwice, Poland;

    Inst Met Zelaza, K Miarki 12-14, PL-44100 Gliwice, Poland;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号