Fatigue tests were conducted on standard smooth laser metal deposition (LMD) Ti-6.5Al-2Zr-1Mo-1V titanium alloy specimens under three constant-amplitude stresses. The mixed failure behaviors and the influence of internal pores on the fatigue life were discussed in detail. The double-peak characteristics of the fatigue life distribution have been observed, and a bimodal lognormal distribution (BLG) with five variables can be used to describe the fatigue life variation. A parameter estimation method based on the maximum likelihood estimation (MLE) method was proposed to estimate the BLG distribution parameters, and the Newton–Raphson algorithm was used to solve the nonlinear equations derived from the likelihood functions. A P-S-N curve description of LMD titanium alloy was established based on the BLG and verified by fatigue life data obtained from a fatigue test.
机译:在三个恒定振幅应力下,对标准的光滑激光金属沉积(LMD)Ti-6.5Al-2Zr-1Mo-1V钛合金试样进行了疲劳测试。详细讨论了混合破坏行为和内部孔隙对疲劳寿命的影响。已经观察到疲劳寿命分布的双峰特征,并且可以使用具有五个变量的双峰对数正态分布(BLG)来描述疲劳寿命变化。提出了一种基于最大似然估计(MLE)方法的参数估计方法来估计BLG分布参数,并使用Newton-Raphson算法求解由似然函数得出的非线性方程。基于BLG建立了LMD钛合金的P-S-N曲线描述,并通过疲劳试验获得的疲劳寿命数据进行了验证。