A new chelating resin has been synthesized by immobilizing 4–(2–thiazolylazo) resorcinol (TAR) onto styrene divinlybenzene copolymer and examined for on-line solid phase extraction/preconcentration of Cd, Co, Cu, Ni, Pb and Zn in seawater and fish otoliths for determination by inductively plasma mass spectrometry (ICP-MS). A volume of 5.0 mL sample solution was loaded onto the mini column of TAR immobilized resin at 2.0 mL min−1 via a sequential injection system. The optimum pH for multielement preconcentration was around pH 5.5. Recoveries were better than 96% in artificial seawater. Elution was achieved with 1.0 mL of 0.75 mol L−1 HNO3. The resin possesses large sorption capacity ranging from 82.0 µmol g−1 for Pb to 319 µmol g−1 for Cu. The detection limits (3s) varied between 0.0016 µg L−1 (Cd) and to 0.015 µg L−1 (Zn) for preconcentration of 5.0 mL blank solutions (pH 5.5). Relative standard deviation (RSD)for three replicate runs was between 0.3% (Cd) and 6% (Zn) at 1.0 µg L−1 level. The procedure was validated by analysis of Nearshore Seawater certified reference material (CASS–4), and then successfully applied to the determination of the trace elements in fish otoliths (CRM 22) and in coastal seawater and estuarine water samples.
机译:通过将4-(2-噻唑基偶氮)间苯二酚(TAR)固定在苯乙烯二乙烯基苯共聚物上,合成了一种新的螯合树脂,并对其在水中的镉,钴,铜,铜,镍,铅和锌的固相萃取/富集进行了在线检测。电感等离子体质谱法(ICP-MS)测定鱼耳石。通过顺序注射系统将体积为5.0 mL的样品溶液以2.0 mL min -1 加载到TAR固定树脂的微型柱上。多元素预浓缩的最佳pH值约为5.5。人造海水中的回收率优于96%。用1.0 mL 0.75 mol L -1 HNO3洗脱。该树脂具有大的吸附能力,范围从对Pb的82.0 µmol g -1 到对Cu的319 µmol g -1 。对于5.0 mL空白溶液(pH 5.5)的预浓缩,检测限(3s)在0.0016 µg L -1 (Cd)和0.015 µg L -1 (Zn)之间变化)。在1.0 µg L -1 浓度下,三个重复运行的相对标准偏差(RSD)在0.3%(Cd)和6%(Zn)之间。该程序通过分析近岸海水认证参考材料(CASS-4)进行了验证,然后成功地用于测定鱼耳石(CRM 22)以及沿海海水和河口水样品中的痕量元素。