首页> 中文期刊> 《中国化学工程学报:英文版》 >The nature of the deactivation of hydrothermally stable Ni/SiO2–Al2O3 catalyst in long-time aqueous phase hydrogenation of crude 1,4-butanediol

The nature of the deactivation of hydrothermally stable Ni/SiO2–Al2O3 catalyst in long-time aqueous phase hydrogenation of crude 1,4-butanediol

         

摘要

The deactivation of Ni/SiO2-Al2 O3 catalyst in hydrogenation of crude 1,4-butanediol was investigated.During the operation time of 2140 h,the catalyst showed slow activity decay.Characterization results,for four spent catalysts used at different time,indicated that the main reason of the catalyst deactivation was the deposition of carbonaceous species that covered the active Ni and blocked mesopores of the catalyst.The TPO and SEM measurements revealed that the carbonaceous species included both oligomeric and polymeric species with high C/H ratio and showed sheet.Such carbonaceous species might be eliminated through either direct H2 reduction or the combined oxidation-reduction methodologies.

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号