摘要

Nanosized calcium carbonate particles were prepared with a continuous gas-liquid membrane contactor. The effects of Ca(OH)2 concentration, CO2 pressure and liquid flow velocity on the particles morphology, pressure drop and membrane fouling were studied. With rising Ca(OH)2 concentrations, the average size of the particles increased. The effects of Ca(OH)2 concentration and CO2 pressure on particles were not apparent under the experimental conditions. When the Ca(OH)2 concentration and liquid flow velocity were high, or the CO2 pressure was low, the fouling on the membrane external surface at the contactor entrance was serious due to liquid leakage, whereas the fouling was slight at exit. The fouling on the membrane inner-surface at entrance was apparent due to adsorption of raw materials. The membrane can be recovered by washing with dilute hydrochloric acid and reused for at least 6 times without performance deterioration.

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号