Manufacture technique of semi-solid slurry of hypoeutectic Al-Si alloy by low superheat pouring and weak electromagnetic stirring

         

摘要

The semi-solid slurry of hypoeutectic Al-Si alloy was manufactured by low superheat pouring and weak electromagnetic stirring. The effects of pouring temperature and stirring power on the semi-solid slurry making process were investigated. The results indicate that the semi-solid slurry to satisfy rheocasting requirement can be made by a combination of low superheat pouring and weak electromagnetic stirring. The pouring temperature (or superheat) and the stirring power significantly affect the morphology and the size of primary α-Al, while there is no obvious effect of the stirring time on primary α-Al. Compared with the samples made by low superheat pouring without stirring, the nucleation rate, particle morphology and grain size of primary α-Al in A356 Al alloy are markedly improved by a process of applying both low superheat pouring and weak electromagnetic stirring. Under the condition of weak electromagnetic stirring applied, the pouring temperature with low superheat can be equivalently to reach the effectiveness obtained from the even lower pouring temperature without stirring.

著录项

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号