Preparation and Sintering of Nano-Sized W-Ni -Fe Powder by Sol-Spray-Drying Process

机译:溶胶-喷雾干燥法制备纳米W-Ni-Fe粉及其烧结

获取原文
获取原文并翻译 | 示例

摘要

In this paper, less than 50nm nano-sized W-Ni-Fe composite powder was prepared by Sol-Spray-Drying Process. The preparing processes such as sol formation condition, reduction process of the procusor were studied in detail. The powder characteristics and sintering behavior of the powders were also studied. The powder is nearly spherical and it has good sinterability. In comparison with traditional micron mixed powder consisting of same composition, the melting temperature of the second phase lowered about 70 ℃, and the sintering temperature for nearly full densification was about 1390℃, which lowered more than 100℃.The effects of rare earth on sintering of the alloy were discussed.
机译:本文采用溶胶-喷雾干燥法制备了小于50nm的纳米级W-Ni-Fe复合粉末。详细研究了溶胶形成条件,引发剂还原过程等制备过程。还研究了粉末的粉末特性和烧结行为。该粉末几乎是球形的,并且具有良好的烧结性。与相同组成的传统微米混合粉相比,第二相的熔融温度降低了约70℃,几乎完全致密化的烧结温度约为1390℃,降低了100℃以上。稀土对讨论了合金的烧结。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号