Two activated carbons employing Scrap Tire as precursor were produced by using two different activating agents, HCl and H_2SO_4 (fixed impregnation ratio 1:1). Both of activated carbons were allowed by single-step to get difference carbonized at 500, 600 and 700°C in a muffle furnace for 1 h. Activated carbons differed with the physical structure, chemical and adsorption properties which were derived from Scanning Electron Microscope, and N_2 adsorption/desorption isotherms. Batched sorption studies were performed to compare the iodine and methylene blue adsorption properties of two carbons. The carbon materials obtained from sulfuric acid activation of 500°C has BET surface area as high as 1066.70 m~2/g, Methylene blue adsorption and Iodine number of 288.90 and 590.50 mg/g, respectively. The surface area and adsorption properties of carbon produced using sulfuric acid activation were higher than that produced using hydrochloric acid activation. The results suggest the feasibility of the process from the point of view of both porous texture and adsorption yield.
机译:通过使用两种不同的活化剂,HCl和H_2SO_4(固定浸渍比1:1)制备使用作为前体作为前体的两种活性炭。通过单步允许在500,600和700°C中允许的单步均匀允许活化的碳在马弗炉中获得1小时。活性炭与扫描电子显微镜衍生的物理结构,化学和吸附性能不同,以及N_2吸附/解吸等温。进行批量吸附研究以比较两种碳的碘和亚甲基蓝色吸附性能。由500℃的硫酸活化获得的碳材料具有高达1066.70m〜2 / g,亚甲基蓝吸附和碘288.90和590.50mg / g的表面积。使用硫酸活化产生的碳的表面积和吸附性质高于使用盐酸活化产生的碳。结果表明,从多孔质地和吸附收率的角度来看,该过程的可行性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号