Grain Growth, Microstructure and Property of Ultrafine WC-Co Alloy by Spark Plasma Sintering

机译:火花等离子烧结超细WC-CO合金的晶粒生长,微观结构和性能

获取原文

摘要

In order to control WC grain size and get a microstructure with fine grain size during the sintering process, WC grain growth in WC-Co cemented carbide was investigated. The possible reason on the grain growth was showed which includes the normal grain growth (NGG) and the abnormal grain growth (AGG). We adopted the SPS (spark plasma sintering) to sinter nanometer WC-Co powder, the range of temperature was 1100 -1250 °C, the pressure was 40MPa, and sintering time was 5min. In this paper, we discuss the density, hardness, microstructures and grain sizes of the sintered samples. The results showed that during the process sintering WC-Co powder, there are two kinds of growths. XRD investigation of the WC-Co samples spark plasma sintered to full density revealed that no new phase was created. Through the observed microstructure of the sintered samples, we analyzed the reason of the abnormal grain growth of WC grain. The density and hardness of samples were increased with increasing temperature.
机译:为了控制WC晶粒尺寸并在烧结过程中具有细粒尺寸的微观结构,研究了WC-Co硬质合金的WC晶粒生长。显示谷物生长的可能原因,其包括正常的晶粒生长(NGG)和异常晶粒生长(AGG)。我们采用SPS(火花血浆烧结)到烧结纳米WC-CO粉末,温度范围为1100 -1250℃,压力为40MPa,烧结时间为5min。在本文中,我们讨论了烧结样品的密度,硬度,微观结构和晶粒尺寸。结果表明,在烧结WC-CO粉末期间,有两种生长。 WC-CO样品的XRD调查烧结至全密度的火花血浆显示出不产生新阶段。通过观察到烧结样品的微观结构,我们分析了WC晶粒异常晶粒生长的原因。随着温度的增加,样品的密度和硬度增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号