Preparation of spinel-type LiMn_2O_4 Cathode material by melt-impregnation method for lithium-ion rechargeable batteries

机译:用熔融浸渍方法制备尖晶石型LiMn_2O_4阴极材料,用于锂离子可充电电池

获取原文

摘要

Spinel-type LiMn_2O_4 cathode materials were prepared by melt-impregnation method with different Mn sources and characterized by BET, XRD and TEM as well as electrochemical testing. The results demonstrated that the cathode material prepared with CMD as Mn sources has smaller particle size, higher first charge and discharge capacity, poor cyclic performance, whereas the cathode material prepared with EMD as Mn soruce has larger particle size, lower first charge and discharge capacity, better cyclic stability. These can be attributed to difference of Mn sources and specific surface areas and purities of Mn sources.
机译:通过具有不同Mn源的熔融浸渍方法制备尖晶石型LiMn_2O_4阴极材料,并通过BET,XRD和TEM以及电化学测试表征。结果表明,用CMD制备的阴极材料作为Mn源具有较小的粒度,较高的电荷和放电容量,循环性能不良,而用EMD制备的阴极材料作为Mn Soruce具有较大的粒度,第一充放电容量较低,更好的循环稳定性。这些可以归因于Mn源和特定表面积和Mn源的纯度的差异。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号