Waste Glass Dust to Reduce Alkali Silica Reaction

机译:废玻璃粉减少碱二氧化硅的反应

获取原文

摘要

Millions of tons of generated glass are wasted each year and being added to landfills in which glass takes one million years to decompose. Since the wasted glass contains a significant amount of silica, a main component in other supplementary cementitious materials (SCMs), this research focuses on whether waste glass powder can be used to reduce alkali-silica reaction (ASR). The glass powders were created from either a dust collection or by additional crushing, with possible blending of an existing SCM fly ash. In addition, compressive strengths of mortar mixtures with each glass powder or combined with fly ash at varying replacements of cement were also monitored. Other common SCMs were compared to the glass powders and fly ash for ASR mortar performance. The glass dust was more effective at reducing ASR than the crushed glass. With moderately reactive aggregates, all combinations of glass or fly ash at 40 percent replacement of cement were found to be acceptable for ASR resistance. However, all glass powders were also found to reduce strength of the mortar.
机译:每年浪费数百万吨的生成玻璃,并将其添加到垃圾填埋场中,在这些垃圾填埋场中,玻璃需要分解一百万年。由于废玻璃含有大量的二氧化硅,而二氧化硅是其他辅助胶凝材料(SCM)的主要成分,因此本研究着眼于废玻璃粉是否可用于减少碱二氧化硅反应(ASR)。玻璃粉是通过集尘或通过额外的压碎以及可能与现有SCM粉煤灰的掺混而制成的。此外,还监测了在各种水泥替代量下,每种玻璃粉或与粉煤灰混合的砂浆混合物的抗压强度。将其他常见的SCM与玻璃粉和粉煤灰的ASR砂浆性能进行了比较。与粉碎的玻璃相比,玻璃粉尘在降低ASR方面更有效。对于具有中等反应性的骨料,发现以水泥替代40%的玻璃或粉煤灰的所有组合均可耐受ASR。但是,还发现所有玻璃粉都会降低砂浆的强度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号