Use of blended cements is growing rapidly in the construction industry due to economical, ecological and technical benefits. Syria is relatively rich in volcanic scoria. In the study, three types of cement were prepared; one plain Portland cement CEM Ⅰ (control) and two blended cements: CEM Ⅱ/A-P and CEM Ⅱ/B-P (EN 197-1), each of them with three replacement levels of scoria: (10%, 15%, 20%) and (25%, 30%, 35%), respectively. Evaluation of sulfate resistance of mortars containing scoria-based cements was performed in accordance with ASTM C1012. Length measurements were performed up to 52 weeks after immersing the specimens into 5% Na_2SO_4 solution. Drying shrinkage has been evaluated using mortar bar method in accordance with ASTM C596. Lengths of mortar bars subjected to drying shrinkage were measured periodically up to 360 days. SRPC cement was employed for comparison in both tests. Test results revealed that the increase of scoria significantly improves the sulfate resistance of mortars. The expansion of scoria-based mortar bars decreased with the increase of scoria replacement level. Further, according to the expansion test results, CEM Ⅱ/B-P can be used instead of SRPC in sulfate-bearing environments. The results of drying shrinkage showed that the CEM Ⅱ/B-P-based mortar bars exhibited greater contraction when compared to the control mortar, especially at early ages. However, the long-term drying shrinkage of mortars was not influenced much by the addition of volcanic scoria.
机译:由于经济,生态和技术优势,建筑行业中混合水泥的使用正在迅速增长。叙利亚火山喷发相对丰富。在研究中,制备了三种类型的水泥。一种普通的波特兰水泥CEMⅠ(对照)和两种混合的水泥:CEMⅡ/ AP和CEMⅡ/ BP(EN 197-1),每种均具有三种代替的渣:(10%,15%,20%)和(25%,30%,35%)。根据ASTM C1012进行了评估,对含有灰渣基水泥的砂浆的耐硫酸盐性进行了评估。将样品浸入5%Na_2SO_4溶液中后长达52周进行长度测量。干燥收缩率已经根据ASTM C596使用砂浆棒法进行了评估。定期测量经受干燥收缩的砂浆棒的长度,直至360天。在两个测试中均采用SRPC水泥进行比较。测试结果表明,氧化渣的增加显着提高了砂浆的抗硫酸盐性。随着灰渣替换量的增加,灰渣基​​砂浆棒的膨胀减少。此外,根据膨胀试验结果,在含硫酸盐的环境中,可以使用CEMⅡ/ B-P代替SRPC。干燥收缩的结果表明,与对照砂浆相比,CEMⅡ/ B-P基砂浆棒表现出更大的收缩率,尤其是在早期。但是,火山灰的加入对砂浆的长期干燥收缩影响不大。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号