The paper describes results from ongoing exposure tests examining steel fibre corrosion in cracked shotcrete. The purpose of the work is to shed light on questions about the long term durability of steel fibres in cracked concrete. In field exposure tests beams with different composition and crack widths are exposed to three different environments. After 2.5 years of exposure there is a continued increase in residual strength noted for small crack widths. For larger crack widths the increase has stopped. Measurements of the chloride contents show higher levels than in an earlier evaluation and the content increases closer to the crack opening. The following conclusions can be drawn from the second evaluation: 1) Samples exposed to freeze-thaw salts show greater evidence of fibre corrosion, 2) An increased crack width leads to increased corrosion, 3) Longer fibres corrode more than short ones at the same crack width, 4) The amount of corrosion decreased with an increased depth from the crack opening.
机译:本文描述了正在进行的暴露测试的结果,这些测试检查了开裂喷射混凝土中的钢纤维腐蚀。这项工作的目的是阐明有关开裂混凝土中钢纤维的长期耐久性的问题。在现场暴露测试中,具有不同成分和裂缝宽度的光束暴露于三种不同的环境。暴露2.5年后,对于较小的裂缝宽度,残余强度会持续增加。对于较大的裂缝宽度,停止增加。氯化物含量的测量显示出比早期评估中更高的含量,并且含量更接近裂纹开口。从第二次评估中可以得出以下结论:1)暴露于冻融盐的样品显示出纤维腐蚀的更多证据,2)裂纹宽度增加导致腐蚀增加,3)同一时间更长的纤维比短的纤维腐蚀更多裂纹宽度,4)腐蚀量随裂纹开口深度的增加而降低。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号