Both stabilizer and couple-agent can affect the melt index of composite materials. Moreover, the different varieties of same stabilizer and couple-agents also results in the difference of melt index of composite materials. The result of melt index test showed that, under the test condition of load 21.6 kg and temperature 190 degC, the melt index of bamboo-plastic composite which was added hot stabilizer 'lead salt' is averagely small by 15.84 g/(10 min) than that of hot stabilizer 'rare earth', and that the melt index derived from 1.5 portions of aluminate is averagely small by 15.09 g/(10 min) than that of 1.5 portions of titanate. The result also revealed that the melt index of bamboo-plastic composite using 1.5 portions of titanate as couple-agents is averagely big by 8.94 g/(10 min) comparing with the negative control (without couple-agents), and that the melt index derived from 1.5 portions of aluminate is averagely big by 23.47 g/(10 min) than that of negative control.
机译:稳定剂和偶联剂均可影响复合材料的熔体指数。此外,相同稳定剂和偶联剂的不同品种也会导致复合材料的熔融指数不同。熔融指数测试的结果表明,在21.6 kg的负载和190℃的温度下的测试条件下,添加了热稳定剂“铅盐”的竹塑复合材料的熔融指数平均小了15.84 g /(10 min)。与热稳定剂“稀土”相比,由1.5份铝酸盐得到的熔体指数平均要比1.5份钛酸盐的熔体指数小15.09 g /(10 min)。结果还表明,与阴性对照(不含偶合剂)相比,使用1.5份钛酸酯作为偶合剂的竹塑复合材料的熔体指数平均高8.94 g /(10分钟)。从1.5份铝酸盐中提取的蛋白质平均比阴性对照大23.47 g /(10分钟)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号