Current Understanding of Cracking of Recovery Boiler Primary Air Port Composite Tubes

机译:目前对回收锅炉一次风口复合管开裂的认识

获取原文
获取原文并翻译 | 示例

摘要

Co-extruded 304L stainless steel/SA210 carbon steel tubes have been widely used in the floors and lower walls ofrnblack liquor recovery boilers in order to provide needed corrosion resistance. However, cracking has been found inrnthe stainless steel layer of both floor and wall tubes, and the cracks in the tubes that form primary air port openingsrnhave, in some cases, advanced into the carbon steel portion of the tubes. A few tube failures have been reported, andrnconsequently, there has to be serious concern about the potential for a tube leak with the possibility of an ensuingrnboiler explosion. This research has been conducted to address possible ways to avoid this cracking: changes inrnoperating procedures, use of alternate tube cladding materials, and modification of the air port design. Results havernprovided guidance on reducing the likelihood of tube cracking through selection of materials, air port design, andrnoperational changes.
机译:共挤304L不锈钢/ SA210碳钢管已广泛用于黑液回收锅炉的地板和下壁,以提供所需的耐腐蚀性。然而,已经发现在地板和壁管的不锈钢层中都开裂,并且在某些情况下,形成主要空气口开口的管中的裂缝已经推进到管的碳钢部分中。已经报道了一些管子故障,因此,必须对管子泄漏的可能性以及锅炉随之爆炸的可能性引起严重关注。进行这项研究的目的是为了解决避免破裂的可能方法:更改无齿操作程序,使用替代管壳材料以及修改气口设计。结果为通过选择材料,气孔设计和操作变更来减少管子破裂的可能性提供了指导。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号