Dual-Mode Fluorophore-Doped Nickel Nitrilotriacetic Acid-Modified Silica Nanoparticles Combine Histidine-Tagged Protein Purification with Site-Specific Fluorophore Labeling

机译:双模式荧光团掺杂的镍三氟乙酸镍修饰的二氧化硅纳米粒子结合了组氨酸标记的蛋白纯化与特定位置的荧光团标记

获取原文
获取原文并翻译 | 示例
           

摘要

We present the first example of a fluorophore-doped nickel chelate surface-modified silica nanoparticle that functions in a dual mode, combining histidine-tagged protein purification with site-specific fluorophore labeling. Tetramethylrhodamine (TMR)-doped silica nanoparticles, estimated to contain 700-900 TMRs per ca. 23 nm particle, were surface modified with nitrilotriacetic acid (NTA), producing TMR-SiO_2-NTA-Ni~(2+). Silica-embedded TMR retains very high quantum yield, is resistant to quenching by buffer components, and is modestly quenched and only to a certain depth (ca. 2 nm) by surface-attached Ni~(2+). When exposed to a bacterial lysate containing estrogen receptor a ligand binding domain (ERa) as a minor component, these beads showed very high specificity binding, enabling protein purification in one step. The capacity and specificity of these beads for binding a his-tagged protein were characterized by electrophoresis, radiometric counting, and MALDI-TOF MS. ERa, bound to TMR-SiO_2-NTA-Ni~(++) beads in a site-specific manner, exhibited good activity for ligand binding and for ligand-induced binding to coactivators in solution FRET experiments and protein microarray fluorometric and FRET assays. This dual-mode type TMR-SiO_2-NTA-Ni~(2+) system represents a powerful combination of one-step histidine-tagged protein purification and site-specific labeling with multiple fluorophore species.
机译:我们提出了荧光团掺杂的镍螯合物表面改性的二氧化硅纳米粒子的第一个示例,其以双重模式起作用,将组氨酸标记的蛋白质纯化与位点特异性荧光团标记结合在一起。四甲基若丹明(TMR)掺杂的二氧化硅纳米粒子,估计每ca包含700-900个TMR。用次氮基三乙酸(NTA)对23 nm的颗粒进行表面改性,生成TMR-SiO_2-NTA-Ni〜(2+)。二氧化硅包埋的TMR保留了很高的量子产率,耐缓冲组分的淬灭作用,并通过表面附着的Ni〜(2+)适度淬灭并仅达到一定深度(约2 nm)。当暴露于含有雌激素受体作为配体结合域(ERa)的次要成分的细菌裂解液时,这些珠子显示出非常高的特异性结合,可以一步纯化蛋白质。这些珠结合组氨酸标签的蛋白的能力和特异性通过电泳,放射计数和MALDI-TOF MS表征。在溶液FRET实验以及蛋白质微阵列荧光和FRET分析中,ERa以定点方式与TMR-SiO_2-NTA-Ni〜(++)珠结合,表现出良好的配体结合活性和配体诱导的与共激活因子的结合。这种双模式TMR-SiO_2-NTA-Ni〜(2+)系统代表了一步标记的组氨酸标签蛋白纯化和具有多种荧光团的位点特异性标记的强大组合。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号